BONDERITE C-AD 4215

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-AD 4215

Main features

    Product Description

    BONDERITE® C-AD 4215 AERO is a clear, colorless liquid additive formulated to enhance the cleaning performance of BONDERITE® C-AK 4215 AERO and other alkaline cleaners when difficult-to-remove soils are encountered. Suitable for both spray and immersion cleaning systems, the additive readily dissolves into alkaline cleaning baths, is compatible with ferrous and nonferrous alloys when used with a compatible base cleaner, and rinses cleanly from treated parts with cool to warm water.

    Key Features

    • Cleaning-performance enhancer for BONDERITE® C-AK 4215 AERO and other compatible alkaline cleaners.
    • Low addition rate of only 1–2% by volume minimizes changes to existing cleaning processes.
    • Suitable for spray and immersion systems with recommended air or mechanical agitation for immersion cleaning.
    • Compatible with ferrous and nonferrous alloys when the selected alkaline cleaner is also compatible.
    • Readily soluble and free-rinsing for efficient incorporation into alkaline cleaning baths.

    Applications / Suitable for

    • Enhancing alkaline cleaner performance
    • Spray alkaline cleaning systems
    • Immersion alkaline cleaning systems
    • Cleaning difficult-to-remove soils
    • Ferrous alloy cleaning processes
    • Nonferrous alloy cleaning processes
    Product Family

    BONDERITE C-AD 4215

    Catalog Product

    Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

    TDS, SDS & Technical Documents

    Technical Specifications

    Other Properties
    Storage TemperatureStorage Temperature
    0–40°C °C
    General Properties
    AppearanceAppearance
    Clear, colorless liquid
    Specific GravitySpecific Gravity
    Density: 0.951–0.961 g/mL

    Additional Information

    Technical Properties

    As-Supplied / Before-Processing Properties

    Supplier-published characteristics of BONDERITE® C-AD 4215 AERO.

    Property Value Unit Method / Condition
    Technology Metal Pretreatment — Supplier classification
    Product Type Additive — Supplier classification
    Application Immersion and Spray — Supplier classification
    Appearance Clear, colorless liquid — As supplied
    Density 0.951–0.961 g/mL Typical property
    Flash Point 110 °C Cleveland Open Cup Method
    Storage Temperature 0–40 °C Recommended storage
    Shelf Life 24 months Original unopened packaging
    Technical Properties

    After-Processing / Operating Properties

    Supplier-recommended operating conditions when using BONDERITE® C-AD 4215 AERO with compatible alkaline cleaners.

    Property Value Unit Method / Condition
    Recommended addition level 1–2 % by volume Add after alkaline cleaner is fully mixed
    Operating temperature 60–80 °C Preferred operating range
    Preferred operating temperature 70 °C Supplier recommendation
    Application methods Spray and immersion — Compatible alkaline cleaning systems
    Immersion agitation Air or mechanical agitation recommended — Immersion cleaning
    Rinsing Cool to warm water rinse — Follow rinsing procedure of the selected alkaline cleaner
    Compatibility Ferrous and nonferrous alloys — Provided the base cleaner is compatible with the substrate

    Leading Brands Trust in Our Products and Services

    • Jabil
    • Linxens
    • Magna
    • Medtronic
    • NXP
    • Philips
    • Semikron
    • Teledyne
    • Thales
    • Vishay
    • ZF
    • AMS
    • Apple
    • Audi
    • Broadcom
    • Borgwarner
    • Bosch
    • Eaton
    • Henkel
    • Honeywell
    • Hysol
    • Intel
    Products that Perform|Knowledge that Serves|Service that Delivers