BONDERITE C-AK ETCH 9HL

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-AK ETCH

Main features

  • High-Copper Aluminum Chem-Mill Processing
  • Controlled Immersion Chemical Milling
  • Improved Line Definition and Etch Uniformity

Product Description

BONDERITE® C-AK ETCH 9HL AERO is a specially compounded alkaline liquid chemical milling etchant developed for high-copper aluminum alloys used in the Chem-Mill process. Applied by immersion, it delivers controlled chemical etching for aerospace manufacturing and has also been used successfully on other aluminum alloys. The formulation is designed for use with BONDERITE® C-AD ETCH additives and ALKETCH INHIBITOR L to achieve consistent line definition and etch-factor uniformity during chemical milling operations.

Key features

  • Chemical milling etchant: Developed specifically for Chem-Mill processing of high-copper aluminum alloys.
  • Immersion process compatible: Designed for immersion etching systems using mild-steel process equipment.
  • Process control support: Used with ALKETCH INHIBITOR L to optimize line definition and etch-factor uniformity.

Applications / Suitable for

  • Chemical milling (Chem-Mill) of aluminum components
  • High-copper aluminum alloys
  • Other aluminum alloys where validated by process qualification
  • Immersion chemical milling systems
  • Aerospace metal pretreatment operations
Product Family

BONDERITE C-AK ETCH 9HL

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied characteristics for BONDERITE® C-AK ETCH 9HL AERO.

Property Value Unit Method / Condition
Technology Metal pretreatment — Supplier classification
Product type Alkaline cleaner etchant — Supplier classification
Appearance Brown liquid — As supplied
Density 1.37–1.45 g/mL Typical property
Storage temperature 10–40 °C Original unopened container
Shelf life 24 months Original unopened packaging
Technical properties

After-processing / operating properties

Typical process conditions published for operation of BONDERITE® C-AK ETCH 9HL AERO.

Property Value Unit Method / Condition
Application method Immersion — Process application
Working concentration 14.5 % by volume Fresh make-up solution
Operating temperature 85–90 °C Recommended operating range
Initial N1 value 6 — Fresh solution target
Initial N2 value 2 — Fresh solution target
ALKETCH INHIBITOR L addition 29 mL/L Raises N2 by 1 mL in fresh solution

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers