BONDERITE C-IC SMUTGO

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE C-IC SMUTGO

Main features

  • Chromate-Free Acid Cleaner
  • Ambient Immersion or Spray Processing
  • Low Electrical Surface Resistance

Product Description

BONDERITE® C-IC SMUTGO NC AERO is a chromate-free concentrated acid cleaner formulated to deoxidize and desmut aluminum alloys using immersion or spray processing. It effectively prepares aluminum surfaces prior to anodizing, conversion coating, bonding, or welding while maintaining low electrical surface resistance. The product operates at ambient temperatures, is readily soluble in water, and offers adjustable etch rates through simple bath control. :contentReference[oaicite:0]{index=0}

Key Features

  • Chromate-free formulation for deoxidizing and desmutting aluminum alloys.
  • Suitable for both immersion and spray processing.
  • Operates effectively at ambient temperatures with adjustable etch rates.
  • Readily soluble in water and easy to control by titration.
  • Prepares aluminum for anodizing, conversion coating, bonding, and welding.

Applications / Suitable for

  • Aluminum alloys
  • Deoxidizing
  • Desmutting
  • Anodizing pretreatment
  • Conversion coating pretreatment
  • Bonding preparation
  • Welding preparation
Product Family

BONDERITE C-IC SMUTGO

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product TypeProduct Type
Chromate-free aluminum deoxidizer
Thermal Properties
Operating TemperatureOperating Temperature
10–38°C (50–100°F) °C

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Metal cleaning — Supplier classification
Product type Acid cleaner — Supplier classification
Appearance Brownish liquid — As supplied
pH (as supplied) <1 — As supplied
Processing solution concentration 18–20 % by volume Working bath preparation
Storage temperature -10 to 60 °C Unopened original packaging
Shelf life 24 months Unopened original packaging
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Nominal etch rate 0.5–2.5 µm/h/side Most aluminum alloys
Operating temperature 10–38 °C 50–100°F; optimum approximately 25°C
Processing time 1–10 minutes Depending on alloy, bath condition and temperature
Spray pressure 1.5–2.0 bar Spray systems
Application methods Immersion or spray — Air agitation recommended for immersion
Nitric acid concentration (when required) 50–80 g/L Specific operations

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers