BONDERITE M-ED 1000

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDERITE M-ED 1000

Main features

  • Nickel Acetate-Based Sealing Process
  • Reduced Smut, Powdering, and Yellowing
  • Commercial and Selected Military Anodizing Seal Processes

Product Description

BONDERITE® M-ED 1000 AERO is a liquid nickel acetate-based anodizing seal additive for clear, integral, and two-step electrolytically colored anodized aluminum. The sealing process improves corrosion resistance by penetrating and sealing the pores of the anodic film, while helping reduce smut, powdering, and yellowing commonly associated with anodizing seal operations. It is suitable for commercial and selected military sealing specifications.

Key Features

  • Liquid nickel acetate sealing additive for anodized aluminum.
  • Improves corrosion resistance by sealing anodic film pores.
  • Helps reduce smut, powdering, and yellowing during anodizing seal operations.
  • Suitable for clear, integral, and electrolytically colored anodized aluminum.
  • Meets commercial and selected military sealing requirements.

Applications / Suitable for

  • Clear anodized aluminum
  • Integral colored anodized aluminum
  • Two-step electrolytically colored anodized aluminum
  • Anodizing seal baths
  • Aerospace aluminum finishing
  • Architectural and decorative anodizing
Product Family

BONDERITE M-ED 1000

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product TypeProduct Type
Electrodeposition pretreatment

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Method / Condition
Technology Metal treatment — Supplier classification
Product Type Anodizing additive — Supplier classification
Chemistry Liquid nickel acetate-based seal process — Supplier description
Physical form Liquid — Supplier description
Application Anodized aluminum sealing — Supplier recommendation
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Method / Condition
Working concentration 1.5–2.5 % by volume 2.0% optimum
Operating temperature 77–88 °C 85°C optimum
Sealing time 5–15 minutes 10–12 minutes optimum
Operating pH 5.7–6.0 — 5.8 optimum
Agitation Mechanical agitation or recirculation — Recommended
Filtration Continuous 3–10 micron filtration — Recommended

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers