BONDRITE C-AK MIL-ETCH

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

BONDRITE C-AK MIL-ETCH

Main features

  • Fine Satin or Frosted Etch on Aluminum
  • Low-Foam Alkaline Formulation
  • Scale- and Sludge-Reducing Sequestering Chemistry

Product Description

BONDERITE® C-AK MIL-ETCH AERO Alkaline Cleaner is a granular alkaline etching compound formulated to produce a fine satin or frosted finish on aluminum and its alloys. The product is used as an immersion etch solution during metal surface preparation and develops a low-foam blanket that helps minimize caustic mist during operation. Its sequestering chemistry helps reduce scale and sludge buildup on tanks and heating coils, supporting efficient bath operation and reduced maintenance. 

Key Features

  • Produces a uniform satin or frosted etch on aluminum and aluminum alloys for surface preparation. 
  • Low-foam alkaline formulation helps reduce caustic mist escaping from the etch bath.
  • Outstanding sequestering action minimizes scale and sludge buildup on tanks and heating coils for improved bath efficiency. 

Applications / Suitable for

  • Immersion etching of aluminum and aluminum alloys
  • Surface preparation prior to subsequent finishing processes
  • Aerospace aluminum processing operations, including approved BAC 5786 additive applications where specified.
Product Family

BONDRITE C-AK MIL-ETCH

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product TypeProduct Type
Granular alkaline cleaner and aluminum etchant
Thermal Properties
Operating TemperatureOperating Temperature
37-72; 32 - 43 (for BAC 5786) °C

Additional Information

Technical properties

As-supplied / before-processing properties

Documented product form and recommended bath-preparation and operating conditions. Conditions should be established and controlled for the specific aluminum-processing application.

Property Value Unit Method / condition
Product form Granular alkaline product — As supplied
Bath preparation 25–50 lb/100 gal General bath buildup
Operating concentration 4–8 (30–60) oz/gal (g/L) General operation and control
Operating temperature 100–160 (37–72) °F (°C) General operation; maintain the established temperature within ±5°F
Treatment time 5–10 minutes Optimum documented treatment time
BAC 5786 concentration 3–5 (22.5–37.5) oz/gal (g/L) Approved for BAC 5786 use as an additive only
BAC 5786 operating temperature 90–110 (32–43) °F (°C) BAC 5786 operation; optimum time 5–10 minutes

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers