COOLTHERM EP-301

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM EP-301

Main features

  • 1.3 W/(m K) Thermal Encapsulation
  • High-Fluidity Intricate-Circuitry Potting
  • 19.7 kV/mm Dielectric Strength

Product Description

CoolTherm® EP-301 AD Epoxy Resin is a general-purpose, thermally conductive epoxy resin formulated for use with CoolTherm® EP-6010 Hardener. The two-component system combines high fluidity and air-release characteristics with a typical cured thermal conductivity of 1.3 W/m·K, supporting the potting of intricate circuitry and encapsulation of power devices. Available as a black or white liquid, the resin has a typical viscosity of 10,350 cP at 25 °C. When mixed with EP-6010 Hardener at 100:5.3 by weight, it cures to a rigid, electrically insulating material with dimensional stability from -65 to 155 °C.

Key features

  • Thermally conductive encapsulation: Provides a typical cured thermal conductivity of 1.3 W/m·K when used with CoolTherm EP-6010 Hardener.
  • High-fluidity epoxy system: Supports air release and material flow when potting intricate circuitry or encapsulating power devices.
  • Electrical and temperature performance: Provides a typical dielectric strength of 19.7 kV/mm and dimensional stability from -65 to 155 °C.

Applications / Suitable for

  • Potting intricate circuitry
  • Encapsulating power devices
  • Thermally conductive epoxy castings up to 200 g
Product Family

COOLTHERM EP-301

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Black or White Liquid
Specific GravitySpecific Gravity
1.88
Physical Properties
ViscosityViscosity
10350 mPa.s
Electrical Properties
Dielectric StrengthDielectric Strength
19.7 kV/mm
Volume ResistivityVolume Resistivity
1 x 10^15 Ohms⋅cm
Thermal Properties
Thermal ConductivityThermal Conductivity
1.3 W/m.K
Mechanical Properties
ElongationElongation
at Break 1.7 %
Chemical Properties
Moisture absorptionMoisture absorption
10 days @25°C 0.2 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of CoolTherm EP-301 AD resin and the mixed EP-301 AD/EP-6010 system before cure. Values are not intended for specification purposes.

Property Value Unit Method / condition
Appearance Black or white liquid — CoolTherm EP-301 AD resin
Viscosity 10,350 cP Resin at 25 °C; test method not stated
Specific gravity 1.88 — Resin at 25 °C
Mix ratio 100:5.3 By weight EP-301 AD resin : EP-6010 hardener
Working life 2 hours Mixed system at 25 °C
Cure time 24 or 2 hours 24 hours at 25 °C or 2 hours at 65 °C after the material reaches the target temperature
Shelf life 1 year From date of manufacture when stored at 25 °C in the original, unopened container

 

Technical properties

After-processing / final-state properties

Typical properties of the EP-301 AD and EP-6010 system after curing for 2 hours at 65 °C followed by 2 hours at 100 °C. Values are not intended for specification purposes.

Property Value Unit Method / condition
Thermal conductivity 1.3 W/m·K Cured bulk material; test method not stated
Dimensional-stability temperature range -65 to 155 °C Documented dimensional-stability range; retained individual properties are not stated
Hardness 87 Shore D Test method not stated
Tensile strength 68 (9,890) MPa (psi) At 25 °C; test method not stated
Coefficient of linear thermal expansion 26 ppm/°C Temperature region and test method not stated
Volume resistivity 1 × 1015 ohm-cm At 25 °C; test method not stated
Dielectric strength 19.7 (500) kV/mm (V/mil) Specimen thickness and test method not stated
Moisture absorption 0.2 % After 10 days at 25 °C; exposure medium and test method not stated

 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers