COOLTHERM SC-6705

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

COOLTHERM SC-6705

Main features

  • 55 to 205 deg C Service Range
  • 2,500 cP Mixed Viscosity
  • 17.7 kV/mm Dielectric Strength

Product Description

CoolTherm® SC-6705 Silicone Encapsulant is a two-component, addition-cure silicone system designed for applications requiring flexible encapsulation and high-temperature service. The resin and hardener mix at a 1:1 ratio by weight or volume to form a black liquid with a typical mixed viscosity of 2,500 cP at 25°C. After cure, the material forms a flexible elastomer with a documented operating-temperature range of -55°C to +205°C, typical thermal conductivity of 0.35 W/m·K, and electrical insulating properties.

Key features

  • Broad operating-temperature range: Suitable for parts and devices operating from -55°C to +205°C.
  • Low mixed viscosity: Provides a typical mixed viscosity of 2,500 cP at 25°C for encapsulation processing.
  • Flexible electrical insulation: The cured system provides 100% elongation at break, typical dielectric strength of 17.7 kV/mm, and volume resistivity of 1 × 1014 ohm-cm at 25°C.

Applications / Suitable for

  • Flexible silicone encapsulation requiring high-temperature service
Product Family

COOLTHERM SC-6705

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Resin: Black Liq | Hardener: Off white Liq | Mixed: Black Liq
Specific GravitySpecific Gravity
1.35
Physical Properties
Viscosity (Part A)Viscosity (Part A)
(Resin) 3000 mPa.s
Viscosity (Part B)Viscosity (Part B)
(Hardener) 2900 mPa.s
Thermal Properties
Thermal ConductivityThermal Conductivity
0.35 W/m.K
Mechanical Properties
ElongationElongation
at break 100 %
Electrical Properties
Dielectric StrengthDielectric Strength
17.7 kV/mm
Volume ResistivityVolume Resistivity
1 x 10^14 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of CoolTherm SC-6705 resin, hardener, and mixed encapsulant before cure. Values are not intended for specification purposes.

Property Value Unit Method / condition
Appearance Black liquid / Off-white liquid / Black liquid — Resin / hardener / mixed system
Viscosity 3,000 / 2,900 / 2,500 cP Resin / hardener / mixed system at 25°C; test method not stated
Specific gravity 1.35 / 1.35 / 1.35 — Resin / hardener / mixed system; test conditions not stated
Mix ratio 1:1 Resin:hardener By weight or volume
Working life 1–2 hours Mixed system at 25°C; endpoint definition and test method not stated
Cure schedule 2 hours / 24 hours — At 65°C / room temperature; time begins after the material reaches the target temperature
Shelf life 6 months Each component when stored at 25°C in the original, unopened container
Technical properties

After-processing / final-state properties

Typical cured properties of CoolTherm SC-6705 Silicone Encapsulant. The source does not state the cure schedule used to prepare the cured-property specimens. Values are not intended for specification purposes.

Property Value Unit Method / condition
Operating temperature range -55 to +205 °C Documented range for parts and devices; retained-property data are not stated
Thermal conductivity 0.35 W/m·K Test method and temperature not stated
Hardness 60 Shore A Test method not stated
Tensile strength 2.07 (300) MPa (psi) Test method and test temperature not stated
Elongation at break 100 % Test method and test temperature not stated
Volume resistivity 1 × 1014 ohm-cm At 25°C; ASTM D257
Dielectric strength 17.7 (450) kV/mm (V/mil) ASTM D149; specimen thickness not stated
Dielectric constant 3.2 — At 100 Hz; ASTM D150
Dissipation factor 0.005 — At 100 Hz; ASTM D150

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers