EPOCAST 1635

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

EPOCAST 1635

Main features

  • High-Temperature Composite Repair
  • High-Strength Aluminum-Filled Epoxy
  • Fatigue-Resistant Epoxy Syntactic

Product Description

EPOCAST® 1635 A/B is a two-component, aluminum-filled epoxy syntactic developed for refilling mis-drilled holes in composite parts. The high-viscosity system combines compressive strength with fatigue resistance under load at elevated temperature and is documented for performance at temperatures up to 177°C (350°F). It mixes at 100:23 by weight or 4:1 by volume and provides a gel time greater than 60 minutes for a 100 g mass at 25°C. The mixed material is blue-gray and may be hand mixed or dispensed from a 4:1 dual-barrel cartridge. EPOCAST® 1635 A/B is qualified to BMS 5-28, Type 31.

Key features

  • Elevated-temperature strength: Provides 12 ksi compressive strength when tested at 177°C under either of the listed cure schedules.
  • Controlled processing: Offers a gel time greater than 60 minutes at 25°C and supports manual mixing or 4:1 cartridge dispensing.
  • Qualified repair material: Designed for refilling mis-drilled holes in composite parts and qualified to BMS 5-28, Type 31.
Product Family

EPOCAST 1635

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Blue-Gray
Density (g)Density (g)
1.8 g/cm3
Mix RatioMix Ratio
100:23
Physical Properties
ViscosityViscosity
100000 mPa.s
Viscosity (Part A)Viscosity (Part A)
300000 mPa.s
Viscosity (Part B)Viscosity (Part B)
50000 mPa.s

Additional Information

Technical properties

As-supplied / before-processing properties

Typical property and processing values for EPOCAST® 1635 A resin, 1635 B hardener, and the mixed system. Values are not guaranteed specifications unless specifically identified.

Property Value Unit Method / condition
Appearance Resin: blue-gray; hardener: amber-gray; mixed: blue-gray — Visual
Density Resin: 1.8; hardener: 1.7; mixed: 1.8 g/cm³ ASTM D1622 at 25°C
Viscosity Resin: >300,000; hardener: >50,000; mixed: >100,000 cP ASTM D2196 at 25°C
Mix ratio 100:23 by weight; 4:1 by volume Parts 1635 A resin to 1635 B hardener
Gel time >60 min 100 g mass at 25°C
Extrusion rate >90 g/min 80 psig at 25°C
Typical cure cycle 7 days at 25°C or gel at 25°C followed by 150 minutes at 93°C — Typical cure schedule
Shelf life 18 months From date of manufacture in original sealed containers stored dry at 4–32°C
Technical properties

After-processing / final-state properties

Typical cured-material results obtained using production batches and standard test methods. Values are representative laboratory data and do not constitute a product specification.

Property Value Unit Method / condition
Compressive strength 15 ksi ASTM D695; tested at 25°C after seven days at 25°C
Compressive strength 12 ksi ASTM D695; tested at 177°C after seven days at 25°C
Compressive strength 25 ksi ASTM D695; tested at 25°C after 2.5 hours at 93°C
Compressive strength 12 ksi ASTM D695; tested at 177°C after 2.5 hours at 93°C
Fluid weight gain — deionized water <1.0 % ASTM D543-87
Fluid weight gain — Skydrol 500B hydraulic fluid <1.0 % ASTM D543-87; BMS 3-11 Type IV, Class 1, Grade A fluid
Fluid weight gain — MIL-PRF-5606 hydraulic fluid <1.0 % ASTM D543-87
Fluid weight gain — TT-S-735 Type III reference fuel <1.0 % ASTM D543-87

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers