EPOCAST 1652

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

EPOCAST 1652

Main features

  • Low Density Syntactic
  • Paste Consistency for Application
  • High Compressive Strength

Product Description

EPOCAST 1652-A/B is a two-component, low-density epoxy syntactic with a thick paste consistency for core filling, core splicing and localized structural reinforcement. The mixed system has a typical density of 0.8 g/cm³ and uses a 100:12 resin-to-hardener mix ratio by weight. It cures at room temperature or with an elevated-temperature post-cure and develops typical compressive strength of 55 MPa at 25°C. Documented applications include adding stiffness and strength to fabricated structures, including helicopter rotor blades, and reinforcing radii and corners in reinforced-plastic structures.

Key features

  • Low-density syntactic system: The mixed material has a typical density of 0.8 g/cm³.
  • Thick paste consistency: The semi-paste mixed form is suited to core filling, core splicing and localized structural build-up.
  • Temperature-dependent compressive performance: Typical compressive strength at 2% strain ranges from 65.5 MPa at −55°C to 4.5 MPa at 177°C.

Applications / Suitable for

  • Core filling for metal-skinned structures
  • Core splicing
  • Adding stiffness and strength to fabricated parts, including helicopter rotor blades
  • Strengthening radii and corners in reinforced-plastic structures
Product Family

EPOCAST 1652

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Light Tan
Density (g)Density (g)
0.8 g/cm3
Mix RatioMix Ratio
100:12

Additional Information

Technical properties

As-supplied / before-processing properties

Typical component and mixed-system properties. Component identity, test temperature and applicable test method are retained where available.

Property Value Unit Method / condition
Color Part A: light tan; Part B: amber; mixed system: light tan — Visual
Density Part A: 0.80; Part B: 1.00; mixed system: 0.8 g/cm³ ASTM D1622
Viscosity / consistency Part A: paste; Part B: 500; mixed system: semi-paste cP where numerical ASTM D2196 at 25°C
Mix ratio 100:12 Parts by weight EPOCAST 1652-A resin to EPOCAST 1652-B hardener
Gel time 30–60 Minutes 100 g mass at 25°C; ASTM D2471
Cure schedule 7 days at 25°C, or gel at 25°C followed by 2–3 hours at 66°C — Room-temperature or elevated-temperature cure option
Storage and shelf life 1 year — Store dry in sealed original containers at 2–40°C, protected from direct sunlight; shelf life applies under supplier standard certification
Technical properties

After-processing / final-state properties

Typical cured properties and laboratory test results; not for specification purposes. Values must be interpreted with the stated test temperature, strain condition, substrate and method.

Property Value Unit Method / condition
Compressive strength at 2% strain 65.5 MPa ASTM D695 at −55°C; 9.50 ksi
Compressive strength at 2% strain 55 MPa ASTM D695 at 25°C; 8.00 ksi
Compressive strength at 2% strain 27.6 MPa ASTM D695 at 83°C; 4.00 ksi
Compressive strength at 2% strain 4.5 MPa ASTM D695 at 177°C; 0.65 ksi
Ultimate compressive strength 62 MPa At 25°C; 9.00 ksi
Tensile lap shear strength 4.8 MPa ASTM D1002; etched aluminum-to-aluminum at 25°C; 700 psi

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF