Hysol GR9810-1P | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

GR9810-1P Epoxy Mold Compound Selector GuideHysol GR9810-1P | Black Epoxy Mold CompoundGR9810-1P Epoxy Mold Compound TMA curve

Main features

  • For sensors & modules
  • Advanced warpage control
  • Reliability and wire sweep control

Product Description

Hysol GR9810-1P is a heat curable, state of the art, black, semiconductor epoxy molding compound developed to meet the stringent encapsulation requirements of package on package (POP and SCSP). It has been formulated to provide the best possible moldability and as wide a molding latitude as possible. It is a Green, halogen free product with, excellent dimensional stability, low shrinkage and High Tg.

Hysol GR9810-1P and its related product GR9810-1PF offer a new technology platform on which Hysol develops epoxy mold compounds for high reliability sensors and modules such as humidity and temperature sensors. Key features of GR9810-1P are summarized as below. 

Reliability

  • Improved adhesion promoter and toughening system
  • High filler loading (>85%) for lower moisture uptake
  • Reduced moisture uptake for best MSL performance

Warpage Control 

  • Multifunctional resin hardener system with high Tg 
  • High cross-linking degree with special toughening system
  • High filler loading for low CTE to minimize thermal mismatch
  • High performance stress modifier to reduce internal stress

Wire Sweep Control

  • Optimized filler PSD with 75um (-1P) or 45um (-1PF) filler cut
  • Low viscosity resin and latent catalyst for ultra long flow

Hysol GR9810-1P is developed for advanced reliability control. The goal of this technology platform is to introduce an epoxy mold compound capable of passing MSL1 260°C on some devices and at least MSL3 260°C on a stacked CSP (PoP) devices. Check reliability test results and typical application Humidity Sensor. 

Product Family

HYSOL GR9810-1P

1. Select Product Form
2. Select Pellet Size
3. Select Pellet Weight
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Product Form, Pellet Size and Pellet Weight.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Black
Filler ContentFiller Content
85 %
Specific GravitySpecific Gravity
1.95
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
170 °C
Thermal ConductivityThermal Conductivity
0.9 W/m.K
UL 94 RatingUL 94 Rating
V-0
Chemical Properties
Moisture absorptionMoisture absorption
0.27 %
Physical Properties
Spiral Flow @ 175°CSpiral Flow @ 175°C
150 cm
Curing Conditions
Transfer PressureTransfer Pressure
30 - 60 kg/cm2
Transfer TimeTransfer Time
15 - 20 s

Additional Information

 GR9810-1P Internal Test Results

1. GR9810-1P has passed MSL3 3 x 260°C reliability test on large device.

2. GR9810-1P has high Tg and high temperature stability.

 

3. GR9810-1P has low viscosity and long flow for wide process window. 

GR9810-1P Customer's Application 

Sensor devices (such as our Smartlinq USB Temperature Data Loggers or our other Temperature Data Loggers) require precise, reliable and cost-effective humidity measurement and control. This allows them to be used reliability and effectively in a wide variety of applications such as consumer goods, automotive, logistics and HVAC applications. As such, GR9810-1P:

  • Is used in variety of applications including mobile devices
  • Passes 160ºC high temperature operating tests
  • Passes MSL1& 1000 TC customer reliability
  • Has the best adhesion on PPF lead frames
  • Is compatible with Cavity and Film Assisted Molding process

Digital humidity and temperature sensors

 

 

 

 

 

 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers