LINQSOL EMC-7535MF | Black Epoxy Mold Compound

Harmonization Code : 3907.30.00.85 | Polyacetals, other polyethers and epoxide resins, in primary forms; polycarbonates, alkyd resins, polyallyl esters and other polyesters, in primary forms : Epoxide resins : Other

LINQSOL EMC-7535MF | High Tg Mold Compound

Main features

  • Green molding compound
  • Designed for high-power TO packages
  • High Tg, low water absorption, low modulus, and excellent thermal stability

Product Description

LINQSOL EMC-7535MF is a green epoxy molding compound specifically developed for high-voltage and high-power semiconductor devices. It offers low modulus to meet low-stress requirements. With a high glass transition temperature (Tg = 215 °C), minimal moisture absorption, a high comparative tracking index (CTI = 600 V), and a UL 94 V-0 flammability rating highlighting its adherence to stringent safety standards for high-power semiconductor applications,  EMC-7535MF guarantees strong performance and outstanding reliability.

Overall, LINQSOL EMC-7535MF seamlessly integrates advanced material properties, safety compliance, and superior performance, precisely meeting the stringent demands of high-power semiconductor components such as TO packages. LINQSOL EMC-7535MF finds its niche in high-voltage and high-power discrete packages and power modules, including but not limited to IGBT, TO220, TO247, and other surface mount devices.

LINQSOL EMC-7535MF proved its reliability in customers' small SiC discretes—zero voids, zero delamination on Ni-plated Cu leadframes—even after thermal cycles (−40 °C ↔ +125 °C).

 

Key Features:

  • High-temperature stability with high Tg (215 °C) 
  • Excellent electrical stability due to low ion content and mobility
  • Low stress with low CTE (9 ppm) and low modulus (15GPa)
  • Low moisture absorption and low mold shrinkage (0.22%)
  • Halogen-free (does not contain Br, Sb, P)
  • UL 94 V-0 Flammability 

Application: SiC MOSFETs; TO-package Devices, IGBT Modules

Product Family

LINQSOL EMC-7535MF

1. Select Package Type
2. Select Product Form
3. Select Pellet Size
4. Select Pellet Weight
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
US Shipping in 12 weeks
CA Shipping in 12 weeks
EU Shipping in 12 weeks
Packaging
Please select Package Type, Product Form, Pellet Size and Pellet Weight.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
Black
Filler ContentFiller Content
84 %
Specific GravitySpecific Gravity
1.96
Electrical Properties
Volume ResistivityVolume Resistivity
33000000000000000 Ohms⋅cm
Chemical Properties
Moisture absorptionMoisture absorption
≤ 0.35 %
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
215 °C
Thermal ConductivityThermal Conductivity
0.8 W/m.K
UL 94 RatingUL 94 Rating
V-0
Mechanical Properties
Molded ShrinkageMolded Shrinkage
0.22 %
Curing Conditions
Transfer PressureTransfer Pressure
40-90 kg/cm2
Transfer TimeTransfer Time
10-25 s
Physical Properties
Spiral Flow @ 175°CSpiral Flow @ 175°C
85 cm
ViscosityViscosity
44000 mPa.s

Additional Information

Processing Instructions

  • Before use, let LINQSOL EMC-7535MF reach room temperature for 24 hours. Keep the bag unopened and stored in a dry location with a relative humidity of ≤50% during thawing to prevent moisture contamination. 
  • Use the materials within 72 hours after removing the container from cold storage.

Storage and Handling

LINQSOL EMC-7535MF is available in pressed pellets in a wide range of sizes to meet specific customer needs. To ensure product integrity, keep it away from oxidizing materials. For long-term storage, maintain a cold environment. The shelf life at 5 °C is 183 days.

 

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers