Loctite Ablestik 2116 Non-Conductive Adhesive

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Loctite Ablestik 2116 Non-Conductive Adhesive

Main features

  • Metal/Glass/Ceramic/Plastic Staking and Bonding
  • 30-Minute Pot Life
  • 415 V/mil Dielectric Strength

Product Description

LOCTITE ABLESTIK 2116 is a two-part, solvent-free, non-conductive epoxy adhesive for staking and bonding applications where added mechanical and structural rigidity is required. The mixed adhesive has a typical viscosity of 100,000 mPa·s at 25°C, a 30-minute pot life, and a 100:22 resin-to-hardener mix ratio by weight. Guideline cure schedules are 24 hours at 25°C or 4 hours at 65°C. The product is documented for bonding metals, glass, ceramics, and most plastics and has an operating temperature range of −60 to 130°C. Typical cured properties include Shore D 90 hardness, a 115°C glass transition temperature, and 415 V/mil dielectric strength.

Key features

  • Non-conductive, solvent-free epoxy: Two-part resin and hardener system for staking and bonding applications.
  • Flexible cure options: Guideline cure schedules are 24 hours at 25°C or 4 hours at 65°C, with a typical 30-minute pot life.
  • Electrical insulation properties: Typical cured dielectric strength is 415 V/mil, with volume resistivity of 6 × 1013 Ω·cm at 25°C.

Applications / Suitable for

  • Staking compound applications
  • Bonding assemblies where added mechanical and structural rigidity is required
  • Bonding metals, glass, ceramics, and most plastics
Product Family

LOCTITE 2116

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
ColorColor
milky, translucent
Mix RatioMix Ratio
100:22
Pot LifePot Life
30 minutes
Specific GravitySpecific Gravity
1.26
Thermal Properties
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
115 °C
Operating TemperatureOperating Temperature
-60 to 130 °C
Electrical Properties
Volume ResistivityVolume Resistivity
6x10^13 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical product and mixed-material properties for product evaluation. These values are reference data and are not product specifications.

Property Value Unit Method / condition
Components Two part — Resin & Hardener — As supplied
Color Milky, translucent — As supplied
Mix ratio, Resin : Hardener 100 : 22 by weight Resin : Hardener
Mixed viscosity 100,000 mPa·s (cP) At 25°C; mixed material
Specific gravity 1.26 — Mixed material
Pot life 30 min Typical mixed material
Technical properties

After-processing / final-state properties

Typical cured-material properties for product evaluation. Values are reference data and are not product specifications; lap shear applies to the stated aluminum-to-aluminum test configuration and cure.

Property Value Unit Method / condition
Operating temperature −60 to 130 °C Documented product operating range
Hardness 90 Shore D Typical cured material
Glass transition temperature (Tg) 115 °C Typical cured material
Coefficient of expansion 5.5 × 10−5 cm/cm/°C Typical cured material
Volume resistivity 6 × 1013; 1 × 1010 Ω·cm At 25°C; at 100°C
Dielectric strength 415 V/mil Typical cured material
Dielectric constant / dissipation factor 4.5 / 0.01 — At 1 kHz
Lap shear strength 17 N/mm² Aluminum-to-aluminum; 2,500 psi equivalent; sample cured 1 h at 65°C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers