LOCTITE 592

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

LOCTITE 592

Main features

  • High-Lubricity Thread Assembly
  • Immediate Low-Pressure Seal
  • Elevated Temperature Fluid Resistance

Product Description

LOCTITE® 592™ is a one-component, medium-strength anaerobic thread sealant designed for locking and sealing metal pipes and fittings. The high-viscosity dimethacrylate ester paste provides high lubricity to help prevent galling during assembly, supports immediate low-pressure sealing, and allows fittings to be repositioned shortly after assembly. After cure, it provides resistance to pressure, vibration, automotive fluids, fuels, water, and elevated temperatures in demanding industrial piping applications.

Key features

  • High-lubricity thread sealing: Helps prevent galling on metal pipe threads and fittings during assembly.
  • Immediate low-pressure seal: Properly tightened fittings can seal immediately while allowing short-term adjustment after assembly.
  • Elevated-temperature fluid resistance: Supports industrial threaded connections exposed to oils, fuels, water, transmission fluid, and temperatures up to 204°C.
Product Family

LOCTITE 592

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Thick opaque off white paste
Specific GravitySpecific Gravity
1.21
Physical Properties
ViscosityViscosity
200,000 - 500,000 mPa.s
Thermal Properties
Thermal ConductivityThermal Conductivity
0.1 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties of the uncured material; values are reference data rather than guaranteed product specifications.

Property Value Unit Method / condition
Technology Acrylic — Uncured material
Chemical type Dimethacrylate ester — Uncured material
Appearance Thick, opaque, off-white paste — TDS description
Components One component — No mixing required
Viscosity classification High — Thread-sealing paste
Cure mechanism Anaerobic — Cures when confined between metal surfaces without air
Strength classification Medium — Thread-sealing application
Specific gravity 1.21 — At 25°C; TDS value
Viscosity 200,000–500,000 mPa·s Brookfield RVF, 25°C; spindle 7, 2 rpm
Density 1.08 g/cm³ At 20°C; SDS value
Flash point >100 °C SDS value
Auto-ignition temperature >300 °C SDS value
Technical properties

After-processing / final-state properties

Typical cured-material properties depend on cure time, substrate activity, temperature, joint geometry, surface condition, and test method.

Property Value Unit Method / condition
Coefficient of thermal expansion 80 × 10−6 K−1 ISO 11359-2
Thermal conductivity 0.1 W/(m·K) ISO 8302
Specific heat 0.3 kJ/(kg·K) Typical cured-material property
Breakaway torque ≥5.7 N·m ISO 10964; 3/8 × 24 grade-2 steel nuts and bolts; cured 24 hours at 93.3°C and tested at 22°C
Breakaway torque ≥0.6 N·m ISO 10964; 3/8 × 24 grade-2 steel nuts and bolts; cured 72 hours at 22°C
Maximum typical application temperature 204 °C Typical application limit stated in TDS
Motor-oil resistance 85 % initial strength MIL-L-46152 motor oil at 87°C; 720-hour exposure
Unleaded-gasoline resistance 90 % initial strength At 87°C; 720-hour exposure
Phosphate-ester resistance 85 % initial strength At 87°C; 720-hour exposure
Distilled-water resistance 90 % initial strength At 87°C; 720-hour exposure
Automatic-transmission-fluid resistance 95 % initial strength At 87°C; 720-hour exposure
Brake-fluid resistance 80 % initial strength At 87°C; 720-hour exposure

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF