LOCTITE CAT 14

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

LOCTITE CAT 14

Main features

  • Powdered Anhydride Epoxy Hardener
  • Long Epoxy Working Life
  • 3-Hour Cure at 150 deg C

Product Description

Henkel LOCTITE® Catalyst 14 is a powdered epoxy hardener (anhydride-based catalyst) designed for use with LOCTITE STYCAST® epoxy encapsulation, potting and casting systems. The catalyst provides excellent high-temperature performance, long working life and superior chemical resistance, making it suitable for electronic encapsulation, electrical insulation and high-reliability industrial applications. Catalyst 14 is commonly used where extended pot life and elevated-temperature service capability are required.

Key Features & Benefits

  • Powdered epoxy hardener for STYCAST epoxy systems.
  • Excellent chemical resistance after cure.
  • High-temperature performance up to 180°C continuous service.
  • Long pot life and extended work life.
  • Suitable for encapsulation, casting and potting applications.
  • Provides durable thermal and electrical performance.
  • Heat-cure chemistry for demanding environments.

Recommended Applications

  • Electronic component encapsulation.
  • Electrical potting and insulation systems.
  • High-temperature epoxy casting applications.
  • Industrial and aerospace electronic assemblies.
  • Chemically resistant epoxy systems.
Product Family

LOCTITE CAT 14

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Product Type Powdered Epoxy Hardener — LOCTITE CAT 14
Chemical Type Anhydride — Epoxy curing agent
Appearance White Powder — As supplied
Density 0.77 - 0.79 g/cm³ 25°C
Physical Form Powder — Free-flowing hardener
Relative Catalyst Usage 2.5 × Catalyst 9 Reference mix ratio basis
Pot Life (100 g @ 25°C) 24 hours Typical value
Shelf Life 1 year Unopened container at room temperature
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Recommended Cure Schedule 3 hours 150°C heat cure
Continuous Service Temperature 180 °C Typical cured system performance
Intermittent Service Temperature 200 °C Typical cured system performance
Chemical Resistance Excellent — Cured epoxy system
High Temperature Performance Excellent — Heat-cured epoxy systems
Working Life Long — Compared with amine-cured systems
Thermal Shock Resistance Good — Depending on resin system used
Primary End Use Encapsulation & Potting — Electronic and electrical assemblies

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers