LOCTITE CAT 27-1

Harmonization Code : 8529.90 | Parts solely or principally used for TV, radio, and transmission

LOCTITE CAT 27-1

Main features

  • Low-CTE Cured Epoxy
  • Two-Hour Working Time
  • Chemical-Resistant Cured Epoxy

Product Description

LOCTITE® CAT 27-1 is a high-performance epoxy hardener designed for use with LOCTITE STYCAST® 2850 MT encapsulation systems. The catalyst is engineered for applications requiring high thermal conductivity, excellent electrical insulation, low coefficient of thermal expansion (CTE), and outstanding thermal shock resistance. It is particularly suitable for high-voltage electronic assemblies, power devices, and encapsulation applications where heat dissipation and long-term reliability under elevated temperatures are critical.

Key Features & Benefits

  • High thermal conductivity for effective heat dissipation.
  • Excellent electrical insulation properties.
  • Low coefficient of thermal expansion (CTE).
  • Long working life and processing window.
  • Excellent chemical resistance.
  • Designed for high-voltage encapsulation and thermal shock environments.
  • Maintains performance at elevated temperatures.

Recommended Applications

  • Electronic component encapsulation.
  • Power electronics and heat-generating assemblies.
  • High-voltage insulation systems.
  • Thermally conductive potting compounds.
  • Industrial electrical equipment requiring thermal shock resistance.
Product Family

LOCTITE CAT 27-1

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical Properties

As-Supplied / Before-Processing Properties

Property Value Unit Condition
Product Type Epoxy Hardener — LOCTITE CAT 27-1
Appearance Brown Liquid — As supplied
Odor Amine-like — Typical
Density 1.05 g/cm³ 25°C
Viscosity 300 mPa·s (cP) 25°C
Mix Ratio 100 : 5 Resin : Hardener By weight
Working Time 2 hours 100 g mass at 25°C
Flash Point >100 °C SDS value
Technical Properties

After-Processing / Final-State Properties

Property Value Unit Condition / Method
Recommended Cure Schedule 4 hours 120°C heat cure
Continuous Operating Temperature -40 to +175 °C Typical service temperature
Intermittent Operating Temperature -40 to +200 °C Typical service temperature
Thermal Conductivity 1.6 W/m·K Cured system
Hardness 94 Shore D Fully cured
Glass Transition Temperature (DMA) 98 °C Tan δ maximum
Surface Resistivity 1.7 × 10¹⁶ Ω Electrical property
Volume Resistivity 4.5 × 10¹⁵ Ω·cm Electrical property
Linear Shrinkage 0.52 % Cured material
Water Absorption (7 Days) 0.09 % Room temperature

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF