MOLYKOTE DX

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE DX

Main features

  • 4,800 N Four-Ball Weld Load
  • 0.10 Press-Fit Friction Coefficient
  • -25 to 125 deg C Service Range

Product Description

MOLYKOTE® DX (S) Paste is a white to off-white, mineral-oil-based grease-paste with lithium soap, white solid lubricants, and a corrosion inhibitor for assembly and long-term lubrication of heavily loaded metallic contacts. It is intended primarily for clean lubrication at low to medium speeds and has a documented service range of -25°C to 125°C. Typical test data include a 4,800 N four-ball weld load, a 0.77 mm wear scar under 800 N for 1 hour, a 0.10 press-fit coefficient of friction with no chatter, and a 0.12 SRV fretting coefficient under the stated test conditions. Apply to clean contact points by brush, spatula, grease gun, automatic device, or central lubrication system.

Key features

  • Clean, light-colored lubrication: White to off-white grease-paste for metallic sliding contacts where visible dark lubricant residue is undesirable.
  • Heavy-load test performance: DIN 51350 four-ball weld load of 4,800 N and Almen-Wieland OK load of 20,000 N.
  • Friction and fretting data: Press-fit coefficient of friction of 0.10 with no chatter and ASTM D7594 SRV fretting coefficient of 0.12.
  • Water and corrosion test results: DIN 51807 static water-resistance rating of 0-90 and DIN 51802 SKF-Emcor corrosion rating of 2 or lower.
  • Flexible application: Suitable for brush, spatula, grease-gun, automatic-device, and central-system delivery.
  • Fluorinated-material statement: Formulated with no intentional PTFE or other PFAS.

Applications / Suitable for

  • Slides, guides, tracks, and other heavily loaded sliding surfaces
  • Plain bearings, bushings, sleeves, and power screw drives
  • Electrical and domestic appliance mechanisms
  • Packaging, office, and precision machinery
  • Textile and plastics-processing machinery
Product Family

MOLYKOTE DX

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Clean, heavy-load assembly and lubricating paste

MOLYKOTE® DX (S) Paste

A light-colored mineral-oil grease-paste with lithium soap, white solid lubricants, and a corrosion inhibitor. It is designed for assembly and long-term lubrication of metallic sliding contacts exposed to heavy loads at low to medium speeds, especially where clean appearance, controlled friction, and resistance to stick-slip or galling are important selection factors.

White solid lubricants NLGI 1-2 -25°C to 125°C 110 mm²/s at 40°C 4,800 N weld load No intentional PTFE or PFAS
Approved product image showing MOLYKOTE DX (S) Paste packaging and label.

MOLYKOTE® DX (S) Paste is a white to off-white grease-paste for clean lubrication of heavily loaded metallic contacts.

As-supplied paste properties

Lubricant system
Mineral oil / lithium soap
White solid lubricants and a corrosion inhibitor support clean, heavily loaded metallic contacts.
Consistency
NLGI 1-2
Current supplier classification; ISO 2137 unworked penetration is 285-315 mm/10.
Base-oil viscosity
110 mm²/s
DIN 51562 value measured at 40°C.
Property Value Unit Method / condition
Product form Grease-paste — Mineral oil, lithium soap, white solid lubricants, and corrosion inhibitor
Color White to off-white — As supplied
Consistency class 1-2 NLGI Current supplier product classification
Unworked penetration 285-315 mm/10 ISO 2137
Density 1.1 g/ml ISO 2811 at 20°C
Base-oil viscosity 110 mm²/s DIN 51562 at 40°C
Service temperature range -25 to +125 °C Supplier-recommended range

Typical values are not specification limits. The documented temperature range does not imply unchanged friction, consistency, wear, or service life throughout the full range.

Load, friction, and protection performance

Four-ball weld load
4,800 N
DIN 51350 part 4 bench result; it is not an equipment load rating.
Press-fit friction
µ 0.10
Typical press-fit result with no chatter under the stated test method.
Water and corrosion
0-90 / ≤2
DIN 51807 static water-resistance rating and DIN 51802 SKF-Emcor corrosion rating.
Property Value Unit Method / condition
Initial break-away torque <300 × 10-3 N·m ASTM D1478-80 at -20°C
Torque after 20 minutes <100 × 10-3 N·m ASTM D1478-80 at -20°C
Flow pressure <500 mbar DIN 51805 Kestemich method at -20°C
Four-ball weld load 4,800 N DIN 51350 part 4
Four-ball wear scar 0.77 mm DIN 51350 part 5; 800 N for 1 hour
Almen-Wieland OK load 20,000 N Almen-Wieland machine
Frictional force 1,560 N Almen-Wieland machine at OK load
Coefficient of friction 0.10; no chatter µ Press-fit test
SRV fretting coefficient 0.12 µ ASTM D7594-10; 100 N, 0.3 mm stroke, 8 hours
Water resistance 0-90 rating step DIN 51807 part 1; static evaluation
Corrosion rating ≤2 degree DIN 51802 SKF-Emcor method
Oil separation ≤3.0 % DIN 51817 standard test

Bench-test values are condition-specific. Preserve the stated method, load, duration, temperature, geometry, and endpoint when comparing products or evaluating an application.

Application process

Apply to clean metallic contact points

Use conventional grease-paste application methods selected for the component geometry and maintenance process. The paste may be applied manually, by automatic lubricating equipment, or through a central lubrication system.

Prepare: Clean the intended points of contact before application.
Apply: Use a brush, spatula, grease gun, or automatic lubricating device according to the assembly and access conditions.
Central delivery: The product is suitable for delivery through a central lubricating system.
Quantity: The supplier permits excess lubrication; establish the practical amount from the contact geometry, motion, cleanliness requirement, and service condition.

 

Storage and Handling

Store between 0°C and 40°C in the original unopened container. Usable life is 60 months from the date of production. Review the current safety data and container label before handling, use adequate ventilation, and avoid contact with strong oxidizing agents.

Applications

Clean, heavy-load lubrication applications

The documented application scope centers on metallic sliding and friction contacts exposed to heavy loads at low to medium speeds. The light-colored paste is particularly relevant where clean appearance and controlled sliding behavior matter alongside load, water-resistance, and corrosion-test performance.

Industrial metal slide, linear guide, and track
Slides, guides, and tracks
For heavily loaded metallic sliding surfaces operating at low to medium speeds. Press-fit and SRV results provide product-specific friction and fretting data for evaluation without establishing universal system performance.
Plain bearing, bushing, sleeve, and power screw
Plain bearings, bushings, sleeves, and power screws
These current supplier-listed use contexts combine sliding contact, assembly, and long-term lubrication. Evaluate the actual material pair, load, speed, contact geometry, and service temperature before specification.
Clean precision machinery mechanism representing electrical, packaging, office, textile, or plastics-processing equipment.
Clean machinery mechanisms
Documented use contexts include electrical and domestic appliances, packaging and office machinery, precision instruments, and textile or plastics-processing machinery where clean low-speed lubrication is required.
Next steps

Evaluate MOLYKOTE® DX (S) Paste for your sliding contact

Krayden can help review the metallic material pair, contact geometry, load, speed, operating temperature, water exposure, cleanliness requirement, application method, and central-lubrication needs for slides, guides, power screws, plain bearings, machinery mechanisms, and related assembly or long-term lubrication applications.

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers