MOLYKOTE HP-870

Harmonization Code : 3403.19 | Lubricating Preparations (With 70% or More Petroleum Oils) For Automotive and Other Uses

MOLYKOTE HP-870

Main features

  • Fully Fluorinated Formulation
  • -20 to 250 deg C Service Range
  • Chemical-Resistant PFPE/PTFE Grease

Product Description

MOLYKOTE® HP-870 Grease is a white, fully fluorinated lubricating grease based on linear perfluoropolyether oil with a PTFE thickener and PTFE solid lubricants. The NLGI Grade 2 formulation combines high-temperature stability, chemical and solvent resistance, corrosion protection, and low base-oil vapor pressure. It is designed for demanding environments including high vacuum, corrosive service, liquefied-natural-gas equipment, cleanrooms, and semiconductor manufacturing equipment where lubricant evaporation can be problematic. Its 350 cSt base-oil viscosity and service-temperature range from −20°C to 250°C support long-term lubrication of bearings, valves, seals, electrical components, plastics, rubbers, and elastomers.

Key features

  • Fully fluorinated formulation: Uses linear PFPE base oil with a PTFE thickener and PTFE solid lubricants.
  • High-temperature capability: Supports service temperatures from −20°C to 250°C.
  • Chemical resistance: Provides resistance to chemicals, solvents, corrosion, and oxidation.
  • Low base-oil vapor pressure: Suitable for high-vacuum and low-volatilization applications.
  • High load-carrying performance: Provides a four-ball weld load greater than 4,900 N under the documented test conditions.
  • Material compatibility: Compatible with most rubber and plastics.

Applications / Suitable for

  • Cleanroom and semiconductor manufacturing equipment
  • High-vacuum and low-volatilization lubrication
  • Corrosive, chemical, and solvent-exposed equipment
  • Liquefied-natural-gas service
  • Rolling-element bearings and hot-air-dryer motor axles
  • Valves, packings, seals, O-rings, plastics, rubbers, and elastomers
Product Family

MOLYKOTE HP-870

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Product TypeProduct Type
Chemically resistant grease; NLGI 2
Specific GravitySpecific Gravity
Approx. 1.9 g/mL at 20°C
Thermal Properties
Operating TemperatureOperating Temperature
−20°C to 250°C °C

Additional Information

Technical properties

As-supplied / before-processing properties

Typical as-supplied characteristics and storage information for MOLYKOTE® HP-870 Grease. Values are not intended as specification limits.

Property Value Unit Method / condition
Technology Perfluoropolyether — Linear PFPE-based grease
Thickener PTFE — Fluorinated-polymer thickener
Solid lubricant PTFE — Supplier-listed composition
Appearance White — Typical property
NLGI grade 2 — Consistency classification
Worked penetration, 60 strokes 280 0.1 mm JIS K 2220
Base-oil viscosity 350 cSt At 40°C
Density 2.0 g/cm³ Typical property
Usable life 36 months Unopened and stored in a cool, dark place
Technical properties

After-application / in-service properties

Typical performance characteristics relevant to the applied lubricant. Results apply only to the stated test methods and conditions.

Property Value Unit Method / condition
Service-temperature range −20 to 250 °C Supplier-listed service range
Bleed 5.0 % MIL-S-8660; 200°C for 24 hours
Evaporation 1.0 % MIL-S-8660; 200°C for 24 hours
Extended evaporation 3.0 % MIL-S-8660; 200°C for 1,000 hours
Four-ball weld load >4,900 N ASTM D2596; 1,500 rpm for 1 minute
Four-ball wear scar 1.3 mm ASTM D2266; 1,200 rpm, 392 N, 1 hour
Low-temperature torque 54 starting / 28 running N·cm JIS K 2220 at −20°C
Emcor corrosion test 0–1 — DIN 51802
Base-oil vapor pressure 2 × 10−6 Pa At 20°C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers