Dow XIAMETER PMX 200

Harmonization Code : 2710199990 |

Dow XIAMETER PMX 200

Main features

  • 1,000 cSt Polydimethylsiloxane Fluid
  • Surface Tension of 21.2 dynes/cm
  • Dielectric Strength of 400 volts/mil

Product Description

XIAMETER™ PMX-200 Silicone Fluid 1000 cSt is a colorless, clear polydimethylsiloxane fluid with a nominal kinematic viscosity of 1,000 cSt. The silicone fluid combines low surface tension with water repellency, heat stability, dielectric performance, and resistance to shear breakdown. Its viscosity-temperature characteristics and chemical stability support use as a lubricant and mechanical fluid, while its spreading and release properties make it suitable for mold release, surface treatment, polish formulations, and foam-control applications.

Key features

  • Stable 1,000 cSt silicone fluid: Provides a nominal kinematic viscosity of 1,000 cSt with resistance to shear breakdown and a viscosity-temperature coefficient of 0.61.
  • Low surface tension and water repellency: A typical surface tension of 21.2 dynes/cm at 25°C supports spreading, wetting, release, and water-repellent performance.
  • Electrical and thermal properties: Provides a typical dielectric strength of 400 volts/mil at 25°C and an open-cup flash point above 326°C.

Applications / Suitable for

  • Elastomer and plastics lubrication
  • Mechanical and damping fluids
  • Electrical insulating fluids
  • Mold release and surface-active applications
  • Automotive, furniture, metal, and specialty polish formulations
  • Foam prevention and foam breaking
Product Family

XIAMETER PMX 200

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Surface TensionSurface Tension
21.2 mN/m
Electrical Properties
Dielectric StrengthDielectric Strength
400 kV/mm
Volume ResistivityVolume Resistivity
1.0x10¹⁵ Ohms⋅cm

Additional Information

Technical properties

As-supplied properties

Typical properties of the 1,000 cSt grade in its supplied fluid state. Values are not intended for use as specification limits.

Property Value Unit Method / condition
Appearance Crystal clear — Typical
Kinematic viscosity 1,000 cSt Nominal grade
Specific gravity 0.970 — At 25°C (77°F)
Refractive index 1.4035 — At 25°C (77°F)
Flash point, open cup >326 (>620) °C (°F) Open cup
Pour point -50 (-58) °C (°F) Typical
Surface tension 21.2 dynes/cm At 25°C (77°F)
Volatile content 0.11 % At 150°C (302°F)
Viscosity-temperature coefficient 0.61 — Typical
Dielectric strength 400 volts/mil At 25°C (77°F)
Volume resistivity 1.0 × 1015 ohm-cm At 25°C (77°F)

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers